Effect of preweld microstructure on HAZ liquation cracking of rene 80 superalloy
Shahsavari, H. A
Effect of preweld microstructure on HAZ liquation cracking of rene 80 superalloy
Shahsavari, H. A ; Sharif University of Technology | 2007
358
Viewed
- Type of Document: Article
- DOI: 10.1179/174328407X179539
- Publisher: 2007
- Abstract:
- The objective of this work was to study the microstructure of as cast, solution treated and overaged Rene 80 superalloy before and after welding treatment. Studies focused on identifying heat affected zone (HAZ) liquation cracking mechanism and the effect of preweld microstructure on it. The formation of HAZ liquation cracking or microfissuring is found to be strongly dependent on constitutional liquation of grain boundary precipitates. These liquated precipitates in the as cast state contain MC carbides and particularly γ/γ' eutectic islands. While in the overaged condition they consist of the MC carbides and borides. Also HAZ grain boundary liquation and subsequent resolidification occur in overaged Rene 80 during welding. MC carbide liquation can be observed at the weldment of solution treated Rene 80 but the intensity of this liquation is not enough for liquid film formation and then cracking. X-ray mapping of MC carbide forming elements, give further evidence on the liquid film formation at hot cracking regions. It shows the enrichment from tungsten and lower amounts of molybdenum and titanium. © 2007 lnatitute of Materials, Minerala and Mining
- Keywords:
- Crack initiation ; Heat affected zone ; Solidification ; Superalloys ; Welding ; X ray analysis ; Constitutional liquation ; Liquation cracking ; Microfissuring ; Microstructure
- Source: Materials Science and Technology ; Volume 23, Issue 5 , 2007 , Pages 547-555 ; 02670836 (ISSN)