Loading...
FEM analysis of single grit chip formation in creep-feed grinding of Inconel 718 superalloy
Zahedi, A ; Sharif University of Technology | 2011
1167
Viewed
- Type of Document: Article
- DOI: 10.4028/www.scientific.net/AMR.325.128
- Publisher: 2011
- Abstract:
- Recent advances in materials science have necessitated the development and understanding of manufacturing processes for safe and repeatable utilization. Grinding is shown to be a promising material removal process especially for brittle and hard to cut materials such as superalloys. Grinding has always been associated with analysis and modeling complications regarding its nature which has limited its extension and reliability of use. The first step in analysis of grinding is considering the action of a single abrasive grit on workpiece surface. In this work the action of a single CBN abrasive grit in creep-feed grinding process of Inconel 718 superalloy is modeled and analyzed using a 3D FEM software, DEFORM. Thermal and mechanical characteristics of the mutual interaction between grit and workpiece surface, and different chip formation phases are defined which can further be used to analyze the whole process
- Keywords:
- CBN abrasive grain ; Superalloy In718 ; Abrasive grains ; Analysis and modeling ; Chip formations ; Creep-feed grinding ; FEM analysis ; Finite Element ; Hard to cut material ; Inconel-718 ; Manufacturing process ; Material removal process ; Mechanical characteristics ; Mutual interaction ; Whole process ; Work pieces ; Abrasives ; Creep ; Finite element method ; Grinding (machining) ; Manufacture ; Reliability analysis ; Three dimensional ; Superalloys
- Source: Advanced Materials Research, 18 September 2011 through 21 September 2011, Stuttgart ; Volume 325 , 2011 , Pages 128-133 ; 10226680 (ISSN) ; 9783037852316 (ISBN)