Determination of the optimum conditions for recovery of gold from zarshuran refractory gold sulfide ore

Aazami, M ; Sharif University of Technology | 2013

3233 Viewed
  1. Type of Document: Article
  2. Publisher: 2013
  3. Abstract:
  4. The orthogonal array design has been used to determine the optimum conditions for gold recovery from Zarshuran refractory gold sulflde ore (Iran) by direct cyanidation and roasting-cyanidation. The Taguchi method was used as the experimental design to determine the optimum conditions of dissolution behavior of gold with cyanidation and roasting-cyanidation from Zarshuran refractory gold ore. The experimental conditions were studied in the range of 10-12 for pH, 20-40 for time(h), 400-1200 for cyanide content (g/ton) and 30 -40 for percent solid(%). Orthogonal array (OA) L9 (34) consisting of four parameters each with three levels, was chosen. From this study for direct cyanidation the total optimum gold dissolution (30.11%) obtained at pH (10), Time (40 h), Cyanide content (800g/ton) and Percent solid (30%). Also for roasting cyanidation the total optimum gold dissolution (34.96%) obtained at pH (12), Time (40 h), Cyanide content (1200g/ton) and Percent solid (35%)
  5. Keywords:
  6. Cyanidation ; Refractory gold ore ; Roasting ; Taguchi method
  7. Source: Iranian Journal of Materials Science and Engineering ; Volume 10, Issue 4 , 2013 , Pages 8-17 ; 17350808 (ISSN)
  8. URL: http://ijmse.iust.ac.ir/browse.php?a_id=603&sid=1&slc_lang=en